One-component adhesive based on the modified vinyl polyacetate dispersion.
After reaching full strength, the joint has a very good adhesion to wood surface subjected to static and dynamic load and offers good initial adhesion.
Applications:
- Bonding solid wood for production of interior joinery;
- Bonding soft wood;
- Bonding hard wood;
- Bonding window joinery bonding floor panels;
- Bonding particle and fibreboard, plywood;
- Bonding other wood-based material;
- Intended for use in cold press or manual bonding;
- Intended for use in hot press for bonding veneer and laminates to particle and MDF boards.
Instructions
Material preparation
The surface to be bonded must be dry cleaned and free from dust, without traces of oils and fats that would impair adhesion. Wood humidity should be 10 to 14 [%]. The elements to be bonded should be matched to each other.
Adhesive application
Stir the adhesive carefully before use. The adhesive can be applied to one or both sides with a brush, spatula, bottle dispenser, applicator, hand roller or machine (using the nozzle or roller). The recommended amount of adhesive applied, depending on the type of surface:
– surface pasting: 80 – 120 [г/м2],
– bonding the mounting: 120 – 150 [г/м2],
– bonding window beams: 150 – 200 [г/м2].
Open time
Open time: 3 ÷ 10 [min]. The open time depends on the wood type, porosity of the wood, humidity and air temperature and the amount of adhesive applied.
Bonding temperature
Use in temperatures 15 [°C] ÷ 30 [°C]. Applies to the ambient temperature, especially the temperature of the material bonded and the adhesive.
Pressing
Pressing pressure — in the range 0.1 to 1.2 [N/mm2] according to the stress occurring in the bonded materials. In case of manual application, the press the surfaces to be bonded together to squeeze out the adhesive excess.
Pressing time — depends on the type of wood and its moisture content, temperature and humidity of air and the amount of adhesive applied, and the stresses occurring in the bonded materials. Press the bonded components until the initial strength is achieved.
Average pressing times suggested:
- Cold press 15 ÷ 30 [min];
- Hot press 2 ÷ 10 [min] (depending on press temperature).
Good results can be achieved wile bonding observing the following conditions:
Bonding temperature | 15 ÷ 25 [°C] |
Relative air humidity | 40 ÷ 70 [%] |
Wood humidity | 10 ÷ 14 [%] |
Amount of adhesive applied | 80 ÷ 200 [g/m2] |
Maximum open time | 3 ÷ 10 [min] |
Cleaning
Wash the tools in water immediately after completing the work. Do not allow the adhesive to dry out. Mechanically remove dried adhesive from tools after soaking in hot water for (about 1 hour).
Packaging
Product is available in 20 kg and 1000 kg plastic containers.
Packaging and transportation are not subject to RID/ADR regulations. Other containers can be provided upon agreement between the manufacture and customer. The packaging may not affect the quality of product.
Storage
Store in original tightly closed containers at temperature range from +5 to +30 [°C]. Product stored in such conditions does not change its properties in the period of 6 months from the date of production.